Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 170 - 190 °C | 338 - 374 °F | |
Multibase TPSiV® 4000-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Nozzle Temperature | 170 - 227 °C | 338 - 441 °F | Average value: 197 °C Grade Count:25 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Nozzle Temperature | 170 - 195 °C | 338 - 383 °F | |
Huntsman AVALON® 80 ABX Thermoplastic Polyurethane Introduction: AVALON 80 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resista.. |
|||
Nozzle Temperature | 170 - 205 °C | 338 - 401 °F | Extrusion |
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 95 R 4813 is a thermoplastic polyester- polyurethane for injection moulding applications. Additional characteristics of the product are very short cycle times and high dimens.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Nozzle Temperature | 170 - 180 °C | 338 - 356 °F | Injection Molding |
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon. |
|||
Nozzle Temperature | 170 °C | 338 °F | |
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colou.. |
|||
Nozzle Temperature | 170 - 190 °C | 338 - 374 °F | |
Huntsman AVALON® 65 AC Thermoplastic Polyurethane Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Nozzle Temperature | 170 - 205 °C | 338 - 401 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4854 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 85 P 4854 is a flame-retardant, halogen-free polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4854 is part.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4694 is a thermoplastic special- polyester-polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and .. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h.. |
|||
Nozzle Temperature | 170 - 200 °C | 338 - 392 °F | Extrusion |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Nozzle Temperature | 170 - 180 °C | 338 - 356 °F | Injection Molding |
Stellarchem MP-835B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |