Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 271 - 338 °C | 520 - 640 °F | Average value: 306 °C Grade Count:3 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |