Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 254 - 332 °C | 490 - 630 °F | Average value: 284 °C Grade Count:18 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Nozzle Temperature | 310 - 332 °C | 590 - 630 °F | |
LTL Color Compounds ColorFast® PCGF120 Polycarbonate, 20% Glass-Filled 20% glass-filled grade, good balance of impact and mechanical propertiesAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 310 - 332 °C | 590 - 630 °F | |
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled 30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |