Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 321 °C | 579 - 610 °F | |
LNP NORYL® EXCP0111 PPS + Polyphenylene Ether, 42% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Nozzle Temperature | 304 - 321 °C | 579 - 610 °F | |
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 327 °C | 580 - 620 °F | |
LTL Color Compounds ColorFast® PC60 Polycarbonate 6 melt extrusion gradeAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 304 - 327 °C | 580 - 620 °F | |
LTL Color Compounds ColorFast® PCGF110 Polycarbonate, 10% Glass-Filled High modulus 10% glass-filled polycarbonate, V2-rated, general purposeAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 332 °C | 580 - 630 °F | |
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 304 - 327 °C | 580 - 620 °F | |
LTL Color Compounds ColorFast® FRPC310 Polycarbonate, Flame-Retarded V0-rated 10% glass-filled polycarbonate, excellent impact strengthAll information provided by LTL Color Compounders, Inc. |