Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 175 °C | 347 °F | |
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | Extrusion |
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80/CF/10/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/BK Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/GY Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80/TF/18/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-0837-1 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7014 Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7112/BK Polyacetal-copolymer, with glass fiber and carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7353/NAT Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7555/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7580 Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7626 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7666/GY Polyacetal-copolymer, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7695 Polyacetal-copolymer, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7713 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7713-NA Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7718 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-7917 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-8082 Polyacetal-copolymer, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-8162 Polyacetal-copolymer, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-8222 Polyacetal-copolymer, with mineral filler, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-8387/EM Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
Lehmann & Voss LUVOCOM® 80-8444 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.dynamic stressReduced moment of inertia compared with metal parts.Isotropic shrinkage character.. |
|||
Nozzle Temperature | 175 - 190 °C | 347 - 374 °F | |
Huntsman AVALON® 70 AE Thermoplastic Polyurethane Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Nozzle Temperature | 175 - 190 °C | 347 - 374 °F | |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Nozzle Temperature | 175 - 190 °C | 347 - 374 °F | |
Lubrizol Estane® T465A Thermoplastic Polyurethane Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |