Polymer Property : Nozzle Temperature = 170 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 165 - 170 °C
329 - 338 °F
Metabolix Mirelâ„¢ F1005 Injection Molding Grade PHA Bioplastic
Mirel F1005 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such..
Nozzle Temperature 165 - 170 °C
329 - 338 °F
Metabolix Mirelâ„¢ F1006 Injection Molding Grade PHA Bioplastic
Mirel F1006 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such..
Nozzle Temperature 165 - 170 °C
329 - 338 °F
Metabolix Mirelâ„¢ P1003 Injection Molding Grade PHA Bioplastic
Mirelâ„¢ P1003 is a general purpose injection molding material with high modulus.Mirel is suitable for a wide range of injection molded food service and packaging applications including caps and ..
Nozzle Temperature 160 - 170 °C
320 - 338 °F
Huntsman IROGRAN® A 60 E 4902 TPU-Polyester
Introduction: IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and molding applications. IROGRAN A 60 E 4902 is part of the HUNTSMAN ..
Nozzle Temperature 165 - 170 °C
329 - 338 °F
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic
Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba..