Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 240 mm/sec | 9.45 in/sec | |
Covestro Bayblend® KU 2-1446 Polycarbonate + ABS Blend
(discontinued **) Key Features:UnfilledPlatableSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bay.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® H950 ABS Novodur H950 is a very high heat injection molding grade with high gloss surface appearanceInformation provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® ET 1100* Polycarbonate + ABS, Mineral Filled As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® ET3036 FR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Extru.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade Injection molding gradegeneral purposecompared to FR 3000 improved chemical resistance and stress cracking behaviorVicat/B 120 temperature = 97 °CUL 94 V-0 at 1.5 mmPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3000 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 97 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | |
Covestro Bayblend® FR 3001 Polycarbonate + ABS Blend Key Features:Flame retarding agentUnfilledFlame retardantSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade Injection molding gradevery easy-flow gradeVicat/B 120 temperature = 96 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3008 HR Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and very good hydrolysis resistance antimony-, chlorine- and bromine-free flame.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3008 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and hydrolysis resistance antimony-, chlorine- and bromine-free flame retardant.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3030 Polycarbonate + ABS, Flame Retardant Grade Flame retardant extrusion gradeVicat/B 120 temperature = 115 °Cgood extrusion and vacuum-forming behaviourUL-listing 94 V-0 (1.5 mm)halogen-free according to DIN VDE 0472-815glow wire temperature (.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3000 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Easy-.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3005 BBS310 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3005 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3006 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3010 IF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3012 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3015 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3040 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® KU 2-1514 BBS073* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeimproved chemical resistance and stress cracking behavior compared to KU 2-1514ball indentation temperature = 125 °CVicat/B 120 tempe.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® M850 XF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® R-FR610 Polycarbonate Recyclate Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame retardantAs of 1 S.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T45 PG Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 112 °Cfor electroplating applicationsPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T50 XF Polycarbonate + ABS Injection molding gradeVicat/B 120 = 115 °Cexcellent flowgood low temperature impact strengthPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T65 AT PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T65 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cgood low temperature impact strengthPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® W85 HI PC ASA Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® W85 XF* Polycarbonate + ASA Developmental product(PC+ASA) blendinjection molding grade with improved weather resistanceoptimized heat ageing stabilityhigh heat resistanceVicat/B 120 = 132 °CPreprocessingMax. Water content |