Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 115 mm/sec | 4.53 in/sec | Injection molding |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
Injection Velocity | 115 mm/sec | 4.53 in/sec | Injection molding |
BASF Petra® 130 FR 30% Glass Filled PET Petra 130 FR is a 30% glass fiber reinforced, flame retardant injection molding polyethylene terephthalate feedstocks. It is recognized as UL 94V-0/5VA by Underwriters Laboratories. It is also avail.. |
|||
Injection Velocity | 115 mm/sec | 4.53 in/sec | Injection molding |
BASF Petra® 140 45% Glass Filled PET Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex.. |
|||
Injection Velocity | 115 mm/sec | 4.53 in/sec | Injection molding |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |