Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 240 mm/sec | 9.45 in/sec | |
Covestro Bayblend® KU 2-1446 Polycarbonate + ABS Blend
(discontinued **) Key Features:UnfilledPlatableSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bay.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Ineos ABS Lustran® ABS M406 Lustran® ABS M406 has very high impact strength and increased chemical and dynamic resistance. It is used for the production of molded plastic articles. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | Injection Molding; ISO 294 |
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® E401 ABS Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® H604 ABS Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® M205FC ABS Novodur HD M205FC is an injection molding grade especially suitable for medical applications providing enhanced stiffness.Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Styrolution Novodur® 5300 ABS Novodur 5300 is a high heat injection molding grade with high impact strength, good chemical resistance and reduced emission (PC modified)Information provided by Styrolution |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® ET3036 FR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Extru.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade Injection molding gradegeneral purposecompared to FR 3000 improved chemical resistance and stress cracking behaviorVicat/B 120 temperature = 97 °CUL 94 V-0 at 1.5 mmPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3000 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 97 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade Injection molding gradevery easy-flow gradeVicat/B 120 temperature = 96 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3020 Polycarbonate + ABS, Mineral Filled 5 % mineral filledfor thin-wall applicationsinjection moldingVicat/B 120 = 103 °CHDT/A = 85 °Cvery good UL listing in small wall thickness (V-0 at 0.75 mm)PreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR 3021 Polycarbonate + ABS, Mineral Filled 15 % mineral filledinjection molding gradeincreased stiffnesstensile modulus = 4800 MPaVicat/B 120 temperature = 98 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame ret.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3000 BBS081 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Impro.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3000 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Easy-.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3009 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3012 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3050 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3100 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® FR3200 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® KU 2-1514 BBS073* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeimproved chemical resistance and stress cracking behavior compared to KU 2-1514ball indentation temperature = 125 °CVicat/B 120 tempe.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T45 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 112 °CPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T50 BBS083 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Goo.. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T65 HI PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature .. |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T65 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cgood low temperature impact strengthPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T65 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® T90 HT Polycarbonate + ABS Injection molding gradehigh heat resistanceVicat/B 120 = 135 °Cball indentation temperature = 125 °Ceasy flowsuitable for supporting life componentsPreprocessingMax. Water content |
|||
Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |
Covestro Bayblend® W85 HI PC ASA Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |