Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 60.0 - 200 mm/sec | 2.36 - 7.87 in/sec | Average value: 107 mm/sec Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Injection Velocity | 60.0 mm/sec | 2.36 in/sec | Injection molding |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Injection Velocity | 60.0 mm/sec | 2.36 in/sec | Injection molding |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Injection Velocity | 60.0 mm/sec | 2.36 in/sec | Injection molding |
Styrolution Terluran® HH-106 ABS Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Injection Velocity | 60.0 mm/sec | 2.36 in/sec | Injection molding |
Styrolution Terluran® HH-112 ABS Terluran HH-112 is an injection molding grade of ABS with very high heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Injection Velocity | 60.0 mm/sec | 2.36 in/sec | Injection molding |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Injection Velocity | 60.0 mm/sec | 2.36 in/sec | Injection molding |
Styrolution Terlux® 2802 TR MABS Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Injection Velocity | 60.0 mm/sec | 2.36 in/sec | Injection molding |
Styrolution Terlux® 2812 TR MABS Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |