Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 20.0 - 30.0 mm/sec | 0.787 - 1.18 in/sec | |
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Velocity | 20.0 - 30.0 mm/sec | 0.787 - 1.18 in/sec | |
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Velocity | 20.0 - 30.0 mm/sec | 0.787 - 1.18 in/sec | |
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Velocity | 20.0 - 30.0 mm/sec | 0.787 - 1.18 in/sec | |
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Velocity | 20.0 - 30.0 mm/sec | 0.787 - 1.18 in/sec | |
Borealis Nepol™ GB601HP Polypropylene, 20% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Injection Velocity | 20.0 - 30.0 mm/sec | 0.787 - 1.18 in/sec | |
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |