Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 275 - 305 °C | 527 - 581 °F | Start Point: 285°C |
Kingfa PA66-C111 Toughened PA66 Features:High impactLow tendency to wrapExcellent balance propertiesApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 275 - 305 °C | 527 - 581 °F | Start Point: 285°C |
Kingfa PA66-G15 15% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Front Barrel Temperature | 275 - 305 °C | 527 - 581 °F | Start Point: 285°C |
Kingfa PA66-G50 50% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Front Barrel Temperature | 290 - 305 °C | 554 - 581 °F | Injection Molding |
LG Chemical LUPOY SC2202 PC+GF20%, High Impact Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 290 - 305 °C | 554 - 581 °F | Injection Molding |
LG Chemical LUPOY SC2302 PC+GF30%, High Impact Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 290 - 305 °C | 554 - 581 °F | Injection Molding |
LG Chemical LUPOY SC3154 PC+GF15% Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide.. |
|||
Front Barrel Temperature | 275 - 305 °C | 527 - 581 °F | Start Point: 285°C |
Kingfa PA66-G30 30% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Front Barrel Temperature | 275 - 305 °C | 527 - 581 °F | Start Point: 285°C |
Kingfa PA66-T15 15% Mineral Filled PA66 Features:Good size stabilityLow tendency to wrapGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower toolsSport applianceInformation Provided by Kingfa Sci. & .. |