Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 288 - 299 °C | 550 - 570 °F | |
Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 288 - 299 °C | 550 - 570 °F | |
Polymer Resources NY6/12-G43 Nylon 612, 43% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Front Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Front Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Front Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Front Barrel Temperature | 288 - 310 °C | 550 - 590 °F | |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1212FR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1212FRR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1212FRRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1212FRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1510FR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1510R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1510R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1510RUV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1510UV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC701 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC703 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC741 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC743 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1212R Molding Grade PC with Release Information provided by Star Plastics, Inc. |