Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LCF50 - PA6 Nylon 6, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF20 - PA6 Nylon 6, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 20% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF30 - PA6 Nylon 6, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-GP1 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Front Barrel Temperature | 271 - 304 °C | 520 - 580 °F | |
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani.. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-IMG33-[color]H Nylon, 33% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-GP4 Modified PPO, General Purpose with HDT of 210 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 271 - 304 °C | 520 - 580 °F | |
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow
(Unverified Data**) Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
LTL Color Compounds ColorFast® PC200 Polycarbonate 20 melt superior processing, fast cyclingAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 271 - 277 °C | 520 - 530 °F | |
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
MRC Polymers NAXELLâ„¢ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity Can be impact modifiedInternal and external lubricant can be addedBlack onlyInformation provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 271 - 299 °C | 520 - 570 °F | |
Wellman Wellamid® GF33-66 XE-N, 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 271 - 299 °C | 520 - 570 °F | |
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-FR7 Modified PPO, V-0 Flame Retardant, Medium Heat, 250 HDT
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
Polymer Resources PPX-FRG10 Modified PPO, UL 94 V-1, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |