Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 441 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 193 - 227 °C
379 - 441 °F
PolyOne Versaflex™ CL2242 Thermoplastic Elastomer (TPE)
Versaflex™ CL2242 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov..
Front Barrel Temperature 193 - 227 °C
379 - 441 °F
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE)
Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov..
Front Barrel Temperature 182 - 227 °C
360 - 441 °F
PolyOne Versaflex™ CL30 Thermoplastic Elastomer (TPE)
Versaflex™ CL30 is an easy processing compound designed for use in injection molding and extrusion applications where water-clarity and excellent colorability are required. - Excellent Clarity - Ex..
Front Barrel Temperature 182 - 227 °C
360 - 441 °F
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE)
Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora..
Front Barrel Temperature 204 - 227 °C
399 - 441 °F
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene..
Front Barrel Temperature 204 - 227 °C
399 - 441 °F
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o..
Front Barrel Temperature 204 - 227 °C
399 - 441 °F
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds..
Front Barrel Temperature 193 - 227 °C
379 - 441 °F
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce..
Front Barrel Temperature 193 - 227 °C
379 - 441 °F
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G2755C Thermoplastic Elastomer (TPE)
Dynaflex™ G2755C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypropylene ..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7430-9001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7430-9001-00 is an easy processing, high performance compound designed for use in applications requiring tough, durable material. - Excellent Heat Stability - Good Ozone and UV Stability..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7980-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7980-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7990-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7990-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-1001-00 can be re..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7990-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7990-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-9001-02 can be re..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7690-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7690-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Front Barrel Temperature 188 - 227 °C
370 - 441 °F
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Copyright © lookpolymers.com All Rights Reserved