Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 240 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact with good flexural stiffness, Custom colorsApplications: Injection molding, Small appliances, Photographic equipmentPerformance grades of polystyrene are engineered to have spe.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 271 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Excellent balance of stiffness, heat resistance, and impact properties, Custom colorsApplications: Injection molding and extrusion, Applications requiring strength and durability where custom colori.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 50 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High strength crystal polystyrene, High heat crystal polystyrene, Custom colorsApplications: Injection molding or extrusion, Designed for applications requiring strength and high heat resistance whe.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 1552 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Easy processing, High modulus, Improve stress whitening, Custom colorsApplications: Injection molding, Office furniture, Electronic media, Photographic equipmentPerformance grades of polystyrene are.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 850 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Custom colorsApplications: Injection molding or extrusion, Suitable replacement for some engineering resins, Toys, Packaging, Business eq.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 765 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, High impact, Color stable, Custom colorsApplications: High flow, multi-purpose injection molding grade where color stability is a requirement, Toys, Appliance, Computer peripheralsPerform.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 782 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Custom colorsApplications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripheralsPerformance grades of polystyrene are engineered to ha.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 8077 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 879 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High heat crystal polystyrene, Color stable, Custom colorsApplications: Injection molding, Designed for applications requiring high strength, high heat resistance, and color stabilityPerformance gra.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova Styrosun® 6600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Front Barrel Temperature | 216 °C | 421 °F | Injection |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
Front Barrel Temperature | 216 - 266 °C | 421 - 511 °F | |
Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consume.. |
|||
Front Barrel Temperature | 216 - 266 °C | 421 - 511 °F | |
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer Elastocon® STK40 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40 is well suited for consumer .. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 8047 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 8049 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High gloss at 60°=95; at 20°C=90, Improved scuff resistance, Custom colorsApplications: Injection molding, Cost effective replacement for some ABS applications, Excellent for applications where hi.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Gas-assist injection moldingThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in laboratory flame tests. L.. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova Zyntar® 351 High Performance Flame Retardant Polystyrene
(discontinued **) High Vicat and heat reflection temperature, Custom colorsApplications: Injection molding, Gas-assist injection molding, Structural foam, TV cabinets, Electronic enclosuresThis is an impact grade of .. |
|||
Front Barrel Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |