Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-GP1 Polyetherimide, General Purpose, Unreinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 343 - 399 °C | 649 - 750 °F | |
LNP ULTEM® SMU6303 Polyetherimide, 5% Glass Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **) Will be UNTW05.Features: Lubricated, High Heat Resistance, Good Wear Resistance, Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provide.. |
|||
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 343 - 399 °C | 650 - 750 °F | |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |