Polymer Property : Front Barrel Temperature = 383 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
Multibase TPSiV® 4100-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr..
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
Multibase TPSiV® 4100-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr..
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
Multibase TPSiV® 4200-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
Multibase TPSiV® 4200-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
Multibase TPSiV® 4200-80A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Front Barrel Temperature 170 - 195 °C
338 - 383 °F
Extrusion
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade
IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially..
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
KEP Kepital® F20 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
KEP Kepital® F20-52 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
KEP Kepital® F30 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
KEP Kepital® FG2025 25% Glass Fiber Reinforced Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 170 - 195 °C
338 - 383 °F
Huntsman AVALON® 65 AC Thermoplastic Polyurethane
Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia..
Front Barrel Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 65 AE Thermoplastic Polyurethane
Introduction: AVALON 65 AE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AE is part of the AVALON Soft Range and offers a premium soling material for casual, sport..
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
Huntsman AVALON® 70 AE Thermoplastic Polyurethane
Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material ..
Front Barrel Temperature 185 - 195 °C
365 - 383 °F
Huntsman AVALON® 75 AE Thermoplastic Polyurethane
Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material ..