Polymer Property : Front Barrel Temperature = 370 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 370 - 395 °C
698 - 743 °F
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding
PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and ..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standar..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. ..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-810 Polyetheretherketone (PEEK)
KetaSpire® KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0.50 kPa-s for standard high-viscosity PEEK grades ..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
KetaSpire® KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry ..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
KetaSpire® KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK)
KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The ..
Front Barrel Temperature 370 °C
698 °F
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir..