Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 232 - 243 °C | 450 - 470 °F | |
Polymer Resources NY6/12-GP1 General Purpose Nylon 612 Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 232 °C | 450 °F | |
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 232 °C | 450 °F | |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 232 °C | 450 °F | |
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 232 °C | 450 °F | |
PTS Trilac® ABS-HF5500 High Flow ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 232 °C | 450 °F | |
LyondellBasell Alathon® M6138 High Density Polyethylene ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness... |
|||
Front Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Front Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Front Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Front Barrel Temperature | 232 °C | 450 °F | |
TPI Porene® ABS-GA800 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 232 °C | 450 °F | |
TPI Porene® ABS-GA803 High Gloss, UV Resistant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 232 °C | 450 °F | |
TPI Porene® ABS-GA850 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 232 °C | 450 °F | |
TPI Porene® ABS-KU650 Super High Heat ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 232 - 260 °C | 450 - 500 °F | |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Front Barrel Temperature | 232 - 260 °C | 450 - 500 °F | |
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose Data provided by Clariant Masterbatches |
|||
Front Barrel Temperature | 232 - 260 °C | 450 - 500 °F | |
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Front Barrel Temperature | 232 °C | 450 °F | |
DuPont Surlyn® 1702SBR
(discontinued **) DuPont™ Surlyn® 1702SBR is a zinc-type resin made from ethylene/methacrylic acid copolymer. This resin has slip, antiblock, and chill roll release additives included in the resin to reduce the coe.. |