Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Middle Barrel Temperature = 68.0 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 1700FC PBT, Unfilled
Celanex 1700FC is a very high molecular weight extrusion grade of unreinforced polybutylene terephthalate for use in food contact applications.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 3300LM PBT, 30% Glass Reinforced
Celanex 3300LM is a 30% glass reinforced lasermarkable grade specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating i..
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
Fortron 1130L4 is a 30% glass-reinforced PPS that has excellent heat and chemical resistance. It is inherently flame-retardant and exhibits high hardness and a good balance of strength and stiffness..
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 4184L4 PPS, 53% Mineral / Glass Reinforced
Fortron 4184L4 is the strongest and toughest glass/mineral reinforced product available. It offers excellent heat resistance at high loads and good chemical resistance. The electrical properties are..
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 6150T6 PPS, 50% Specialty
Fortron 6150T6 is a 50% glass-fiber reinforced and mineral-filled grade with improved impact and heat shock resistance.Information provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 6160B4 PPS, 60% Mineral / Glass Reinforced
Fortron 6160B4 has excellent heat and chemical resistance as well as good electrical properties. This product is inherently flame-retardant and offers high hardness and rigidity. 6160B4 has demonstr..
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 6162A7 PPS, Mineral / Glass Reinforced
Fortron 6162A7 is a mineral/glass reinforced grade for applications requiring the highest flow.Information provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 2521 XAP² ™ LS colored POM, UV Resistant
POM copolymerInformation provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 10/9005 POM, Unfilled
Hostaform« C 9021 10/9005 is a nominal 9 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Hostaform« C 9021 10/9005 can be laser marked wi..
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 SW XAP² ™ LS POM, Tribological
POM copolymerInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese VANDAR 6000 PBT, Unfilled
Vandar 6000 is a toughened polyester alloy with excellent cold temperature impact resistance.Information provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese VECTRA A625 LCP, 25% Specialty
Good wear characteristics. 25% graphite filled.Information provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese VECTRA E440i LCP, 42% Mineral / Glass Reinforced
Mineral and glass filled grade with low warp, easy flow and smooth surface apperance.Information provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese VECTRA MT4350 LCP, 40% Medical Technology
Mineral filled grade with low warp, easy flow and smooth surface appearance.Information provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese VECTRA V143XL LCP, 42% Glass Reinforced
LCP/PPS blend. Maintains most of the characteristics of E130i with improved weldline strength and flatness in certain geometries. 40% glass reinforced.Information provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese ZENITE 7244 LCP, 40% Mineral / Glass Reinforced
Zenite 7244 is a 40% glasslmineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295C, high flow and good flatness."Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 4022 PBT, Specialty
A white PBT resin typically used for applications requiring very opaque parts.Information provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 531HS PBT, Glass Reinforced
Celanex 531HS is a 30% fiberglass reinforced PBT which has an excellent balance of mechanical properties and processability. Celanex 531HS is specifically designed to exhibit excellent thermal shoc..
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON ICE 714A PPS, 65% Mineral / Glass Reinforced
Fortron ICE 714A is a faster crystallizing version of Fortron 6165A4. It offers similar characteristics to the 6165A4 with improved processing that improves crystallization efficiency and reduces cy..
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 TF POM, Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 9021 XAP² ™ POM, Unfilled
POM copolymerInformation provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® XGC25-LW01 POM, 25% Glass Reinforced
Hostaform« XGC25-LW01 is an injection molding grade reinforced with approx. 25% glass fibers and tribological modification for sliding applications requiring low friction and wear.Information provi..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese VANDAR 8000 PBT, Unfilled
Vandar 8000 polyester alloy is designed to meet UL94 V-0 requirements at 1/32 inch thickness while retaining excellent impact resistance. The product is characterized by excellent moldability and su..
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 320 PPS, Unfilled
0320 exhibits a high melt strength for extrusion processes. The material demonstrates excellent heat and chemical resistance. The intended use of this product is for extruding monofilament/fibers, r..
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese FORTRON 6341L4 PPS, 40% Specialty
Fortron 6341L4 is a tribological-modified Fortron«-PPS containing 40% glass fibre. Fortron 6341L4 comprises the same mechanical properties like Fortron 1342L4, but with a different tribological adj..
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® C 2521 G POM, Tribological
Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese CELANEX 4306 PBT, 30% Glass Reinforced
Celanex 4306 is a 30% glass reinforced, toughened, low warpage thermoplastic polyester.Information provided by Celanese
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Celanese Hostaform® MT8U05 POM, Medical Technology
Hostaform« acetal copolymer grade MT8U05 is a special grade developed for medical industry applications containing low residual monomers and no animal products. The material can be identified by U..
Middle Barrel Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Celanese VANDAR 4662Z PBT, 30% Glass Reinforced
Vandar 4662Zis a high impact polyester alloy which contains 30% glass fiber loading. It is characterized by toughness, dimensional stability, and high modulus. Good weatherability and moldability ar..