Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 175 - 195 °C | 347 - 383 °F | |
Huntsman AVALON® 80 ABX Thermoplastic Polyurethane Introduction: AVALON 80 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Middle Barrel Temperature | 170 - 195 °C | 338 - 383 °F | Extrusion |
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a.. |
|||
Middle Barrel Temperature | 170 - 195 °C | 338 - 383 °F | Extrusion |
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe.. |
|||
Middle Barrel Temperature | 175 - 195 °C | 347 - 383 °F | |
KEP Kepital® F20 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 175 - 195 °C | 347 - 383 °F | |
KEP Kepital® F20-52 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 175 - 195 °C | 347 - 383 °F | |
KEP Kepital® F30 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 175 - 195 °C | 347 - 383 °F | |
KEP Kepital® FG2025 25% Glass Fiber Reinforced Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 185 - 195 °C | 365 - 383 °F | Extrusion |
Huntsman IROGRAN® A 91 P 4945 TPU-Polyester Introduction: IROGRAN A 91 P 4945 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 91 P 4945 is part of the HUNTSMAN technical ext.. |
|||
Middle Barrel Temperature | 185 - 195 °C | 365 - 383 °F | Transition, Extrusion |
Stellarchem DIOSHY® MP-960NC TPE Compound This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Middle Barrel Temperature | 185 - 195 °C | 365 - 383 °F | Transition, Extrusion |
Stellarchem LP-830 TPE Compound This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Middle Barrel Temperature | 171 - 195 °C | 340 - 383 °F | |
A. Schulman ComAlloy Voloy® 101 Polypropylene, Impact Modified, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |