Processing Properties Metric English Comments
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and ..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standar..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. ..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-810 Polyetheretherketone (PEEK)
KetaSpire® KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0.50 kPa-s for standard high-viscosity PEEK grades ..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
KetaSpire® KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry ..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
KetaSpire® KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK)
KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK)
KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The ..
Middle Barrel Temperature 365 °C
689 °F
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir..