Polymer Property : Middle Barrel Temperature = 235 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 224 - 235 °C
435 - 455 °F
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 224 - 235 °C
435 - 455 °F
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 224 - 235 °C
435 - 455 °F
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 225 - 235 °C
437 - 455 °F
Injection Molding
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance
Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical
Middle Barrel Temperature 225 - 235 °C
437 - 455 °F
Solvay Technyl® C 206 Nylon 6, EH0
Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f..
Middle Barrel Temperature 225 - 235 °C
437 - 455 °F
Solvay Technyl® C 206 Nylon 6, EH50
Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f..
Middle Barrel Temperature 225 - 235 °C
437 - 455 °F
Compression Zone
Solvay Technyl® C206F Unfilled, Fast Cycle Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Middle Barrel Temperature 225 - 235 °C
437 - 455 °F
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6
Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay.
Middle Barrel Temperature 225 - 235 °C
437 - 455 °F
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant
This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr..
Middle Barrel Temperature 225 - 235 °C
437 - 455 °F
Mid-2. Region Temperature
Tisan TISBLEND® PC/ABS
TISBLEND has a wide area of application in electric/electronic, food packaging, information technology, information technology, medical and automotive industries. General Specification include: High..