Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 218 °C | 424 °F | Extrusion |
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Middle Barrel Temperature | 218 °C | 424 °F | |
Lubrizol Estaloc® 59020 Reinforced Thermoplastic Polyurethane Type: Estaloc® 59020 RETPU is a polyester-type reinforced engineered thermoplastic polyurethane (RETPU).Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.. |
|||
Middle Barrel Temperature | 218 °C | 424 °F | |
Lubrizol ESTALOC® 60155 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol |
|||
Middle Barrel Temperature | 218 °C | 424 °F | |
DuPont Surlyn® 1702SBR
(discontinued **) DuPont™ Surlyn® 1702SBR is a zinc-type resin made from ethylene/methacrylic acid copolymer. This resin has slip, antiblock, and chill roll release additives included in the resin to reduce the coe.. |