Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | >= 140 °C | >= 284 °F | |
Borealis Visico™ LE4481/LE4437 Moisture-Crosslinking Polyethylene Compound for Flexible Low Voltage Insulation Visico LE4481/LE4437 is a natural, low-density ethylene vinyl silane/ ethylene butyl acrylate terapolymer that is designed for flexible low voltage wire insulation and jacketing. The combination of.. |