Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 2.50 min @Temperature 246 °C |
0.0417 hour @Temperature 475 °F |
|
Lord Adhesives Flocklok® 853 Blocked Flock Adhesive Flocklok® 853 is a blocked, heat-curing, single coat adhesive used to adhere polyester or nylon fibers (flock) to a variety of elastomers including EPDM, NR, CR, and SBR. Flocked substrates provi.. |
|||
Cure Time | 2.50 min @Temperature 246 °C |
0.0417 hour @Temperature 475 °F |
|
Lord Adhesives Flocklok® 853A Flock Adhesive LORD Flocklok® 853A is a blocked, heat-curing, singlecoat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates pro.. |
|||
Cure Time | 2.50 min @Temperature 204 °C |
0.0417 hour @Temperature 399 °F |
|
Lord Adhesives Flocklok® 855 Flock Adhesive LORD Flocklok® 855 adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good res.. |
|||
Cure Time | 2.50 min @Temperature 125 °C |
0.0417 hour @Temperature 257 °F |
|
Dow Corning SE 4430 KIT Two-part, thermally conductive elastomer, soft, good thermal conducitvity, UL 94 V-0 rating, low viscosity.Information provided by Dow Corning |
|||
Cure Time | 2.50 min @Temperature 125 °C |
0.0417 hour @Temperature 257 °F |
|
Dow Corning 3-4133 DIELECTRIC GEL KIT Two-part, clear, heat cure, and firm.Information provided by Dow Corning |
|||
Cure Time | 2.50 min @Temperature 125 °C |
0.0417 hour @Temperature 257 °F |
|
Dow Corning 3-4241 DIELECTRIC TOUGH GEL KIT Two-part, translucent green, RT or heat cure, UV indicator, long working time, tough primerless chemical adhesion, UL 94 V-1 flammability classification.Information provided by Dow Corning |
|||
Cure Time | 2.50 min @Temperature 80.0 °C |
0.0417 hour @Temperature 176 °F |
|
Dow Corning 3631 PART A&B KIT Two-part, solvent free, heat-cured liquid silicone rubber.Information provided by Dow Corning |
|||
Cure Time | 2.50 min @Temperature 204 °C |
0.0417 hour @Temperature 399 °F |
|
3M Scotchcast™ 5555 10G Electrical Insulating Epoxy Resin 3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating.. |