Polymer Property : Cure Time = 10.2 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 10.2 min

@Temperature 23.0 °C
0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond HH120 Anaerobic Threadlocker
Permabond® HH120 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Its high viscosity allows for ..
Cure Time 10.2 min

@Temperature 23.0 °C
0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond HL138 Anaerobic Retaining Compound
Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which ..
Cure Time 10.2 min

@Temperature 23.0 °C
0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond HM118 Anaerobic Threadlocker
Permabond® HM118 Threadlocker is an excellent general-purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Cure is fast and reliable on s..
Cure Time 10.2 min

@Temperature 23.0 °C
0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond HM129 Anaerobic Threadlocker
Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st..
Cure Time 10.2 min

@Temperature 23.0 °C
0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond HM161 Anaerobic Retaining Compound
Permabond® HM161 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space’ between parts and upon cure unitiz..
Cure Time 10.2 min

@Temperature 23.0 °C
0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond MM115 Anaerobic Threadlocker
Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance...
Cure Time 10.2 min

@Temperature 23.0 °C
0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond MM115P Pure Anaerobic Threadlocker
Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten..