Polymer Property : Cure Time = 10.0 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 420 - 600 min

@Temperature 25.0 °C
7.00 - 10.0 hour

@Temperature 77.0 °F
4 dry mils; tack free
Lord Adhesives Aeroglaze® 9929 Epoxy Primer
Aeroglaze® 9929 epoxy primer is designed to be used on properly prepared aluminum and steel surfaces for applications that require protection against corrosion.All information provided by Lord.