Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 1.50 min @Temperature 125 °C |
0.0250 hour @Temperature 257 °F |
|
Loctite® Varidot™ 3612 Stencil Print Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te.. |
|||
Cure Time | 1.50 min @Temperature 125 °C |
0.0250 hour @Temperature 257 °F |
|
Loctite® Varidot™ 3614 Stencil Print Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te.. |
|||
Cure Time | 1.50 min @Temperature 125 °C |
0.0250 hour @Temperature 257 °F |
|
Loctite® Varidot™ 3617 Stencil Print Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te.. |
|||
Cure Time | 1.50 min @Temperature 150 °C |
0.0250 hour @Temperature 302 °F |
|
Dow Corning 3-4133 DIELECTRIC GEL KIT Two-part, clear, heat cure, and firm.Information provided by Dow Corning |
|||
Cure Time | 1.50 min @Temperature 125 °C |
0.0250 hour @Temperature 257 °F |
|
Dow Corning 3-4222 DIELECTRIC FIRM GEL KIT Two-part, translucent green, firm, fast RT or heat cure, and primerless chemical adhesion.Information provided by Dow Corning |
|||
Cure Time | 1.50 min @Temperature 125 °C |
0.0250 hour @Temperature 257 °F |
|
Dow Corning 3-4680 SILICONE GEL KIT Two-part, transparent blue, fast RT or heat cure, low viscosity.Information provided by Dow Corning |
|||
Cure Time | 1.50 min @Temperature 232 °C |
0.0250 hour @Temperature 450 °F |
|
3M Scotchcast™ 5555 10G Electrical Insulating Epoxy Resin 3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating.. |
|||
Cure Time | 1.50 min @Temperature 125 °C |
0.0250 hour @Temperature 257 °F |
|
Loctite® Varidot™ 3616 Stencil Print Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te.. |