Processing Properties Metric English Comments
Cure Time 1.50 min

@Temperature 125 °C
0.0250 hour

@Temperature 257 °F
Loctite® Varidot™ 3612 Stencil Print
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te..
Cure Time 1.50 min

@Temperature 125 °C
0.0250 hour

@Temperature 257 °F
Loctite® Varidot™ 3614 Stencil Print
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te..
Cure Time 1.50 min

@Temperature 125 °C
0.0250 hour

@Temperature 257 °F
Loctite® Varidot™ 3617 Stencil Print
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te..
Cure Time 1.50 min

@Temperature 150 °C
0.0250 hour

@Temperature 302 °F
Dow Corning 3-4133 DIELECTRIC GEL KIT
Two-part, clear, heat cure, and firm.Information provided by Dow Corning
Cure Time 1.50 min

@Temperature 125 °C
0.0250 hour

@Temperature 257 °F
Dow Corning 3-4222 DIELECTRIC FIRM GEL KIT
Two-part, translucent green, firm, fast RT or heat cure, and primerless chemical adhesion.Information provided by Dow Corning
Cure Time 1.50 min

@Temperature 125 °C
0.0250 hour

@Temperature 257 °F
Dow Corning 3-4680 SILICONE GEL KIT
Two-part, transparent blue, fast RT or heat cure, low viscosity.Information provided by Dow Corning
Cure Time 1.50 min

@Temperature 232 °C
0.0250 hour

@Temperature 450 °F
3M Scotchcast™ 5555 10G Electrical Insulating Epoxy Resin
3M Scotchcast Electrical Resin 5555 is a one-part, green pigmented, rapid heat curing powder coating. It is designed to provide a continuous, tough moisture and chemical resistant dielectric coating..
Cure Time 1.50 min

@Temperature 125 °C
0.0250 hour

@Temperature 257 °F
Loctite® Varidot™ 3616 Stencil Print
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te..