Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 3.00 - 6.00 MPa | 435 - 870 psi | |
Borealis Daplen™ EG103AI Polypropylene Compound, Mineral Filled Daplen™ EG103AI is a 15 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and high melt flow rate.. |
|||
Hold Pressure | 3.00 - 6.00 MPa | 435 - 870 psi | |
Borealis Daplen™ EG250AI Polypropylene TPO Compound Daplen™ EG250AI is a 20% mineral reinforced impact modified polypropylene compound suitable for injection molding. This material has an excellent balance between impact strength and stiffness, giv.. |
|||
Hold Pressure | 3.00 - 6.00 MPa | 435 - 870 psi | |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Hold Pressure | 3.00 - 6.00 MPa | 435 - 870 psi | |
Borealis HK030U Polypropylene Compound HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit.. |
|||
Hold Pressure | 3.00 - 6.00 MPa | 435 - 870 psi | |
Borealis Daplen™ EE065AI Polypropylene Elastomer Modified Daplen™ EE065AI is an elastomer modified polypropylene with increased crystallinity. This material has an excellent balance between impact strength and stiffness. The product is available in natu.. |
|||
Hold Pressure | 3.00 - 6.00 MPa | 435 - 870 psi | |
Borealis Daplen™ EE189AI Polypropylene TPO Compound Daplen™ EE189AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Hold Pressure | 3.00 - 6.00 MPa | 435 - 870 psi | |
Borealis Daplen™ EF267AI Polypropylene TPO Compound Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Hold Pressure | 3.00 - 6.00 MPa | 435 - 870 psi | |
Borealis Xmod™ GD301FE Polypropylene, Glass Fiber Reinforced Xmod™ GD301FE is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also a.. |
|||
Hold Pressure | 3.00 - 6.00 MPa | 435 - 870 psi | |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |