Polymer Property : Hold Pressure = 80.0 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Hold Pressure 80.0 - 100 MPa
11600 - 14500 psi
Eurotec® Tecoform® PO20 GR10 NL HS POM, 10% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Hold Pressure 80.0 - 100 MPa
11600 - 14500 psi
Eurotec® Tecoform® PO20 GR25 NL HS POM, 25% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Hold Pressure 80.0 - 100 MPa
11600 - 14500 psi
Eurotec® Tecoform® PO20 NL IL POM, impact modified, natural
Information provided by Eurotec®
Hold Pressure 80.0 - 100 MPa
11600 - 14500 psi
Eurotec® Tecoform® PO20 NL RT POM, PTFE modified, natural
Information provided by Eurotec®
Hold Pressure 80.0 - 100 MPa
11600 - 14500 psi
Eurotec® Tecoform® PO30 GB30 NL HS POM, 30% glass bead reinforced, heat stabilized, natural
Information provided by Eurotec®
Hold Pressure 80.0 - 100 MPa
11600 - 14500 psi
Eurotec® Tecoform® PO20 AR10 NL HS POM, 10% aramid fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Hold Pressure 80.0 - 100 MPa
11600 - 14500 psi
Eurotec® Tecoform® PO20 NL RM POM, MoS2 modified, natural
Information provided by Eurotec®
Hold Pressure 80.0 - 100 MPa
11600 - 14500 psi
Eurotec® Tecoform® PO20 NL RW POM, surface modified, natural
Information provided by Eurotec®
Hold Pressure 80.0 - 100 MPa
11600 - 14500 psi
Eurotec® Tecoform® PO30 GB20 NL HS POM, 20% glass bead reinforced, heat stabilized, natural
Information provided by Eurotec®
Hold Pressure 80.0 - 100 MPa
11600 - 14500 psi
Eurotec® Tecoform® PO30 GR20 NL HS POM, 20% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®