Processing Properties Metric English Comments
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 55 AEX Thermoplastic Polyurethane
Introduction: AVALON 55 AEX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 55 AEX is part of the AVALON Perform Range and offers a specially designed,..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 60 ABX Thermoplastic Polyurethane
Introduction: AVALON 60 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 ABX is part of the AVALON Perform Range and offers a specially designed,..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 60 DB Thermoplastic Polyurethane
Introduction: AVALON 60 DB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DB is part of the AVALON Perform Range and offers a premium soling materi..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 60 DE Thermoplastic Polyurethane
Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 80 ABU Thermoplastic Polyurethane
Introduction: AVALON 80 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABU is part of the AVALON Perform Range and offers a premi..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 80 ABX Thermoplastic Polyurethane
Introduction: AVALON 80 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABX is part of the AVALON Perform Range and offers a specially designed,..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane
Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling ..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 98 AE Thermoplastic Polyurethane
Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane
Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 65 AC Thermoplastic Polyurethane
Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 65 AE Thermoplastic Polyurethane
Introduction: AVALON 65 AE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AE is part of the AVALON Soft Range and offers a premium soling material for casual, sport..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 65 DB Thermoplastic Polyurethane
Introduction: AVALON 65 DB is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DB is part of the AVALON Perform Range and offers a premium soling material for sports foo..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 65 DE Thermoplastic Polyurethane
Introduction: AVALON 65 DE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DE is part of the AVALON Perform Range and offers a premium soling material for sports foo..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 65 DEU Thermoplastic Polyurethane
Introduction: AVALON 65 DEU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 65 DEU is part of the AVALON Perform Range and offers a premi..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 70 ABX Thermoplastic Polyurethane
Introduction: AVALON 70 ABX is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a speci..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 75 AE Thermoplastic Polyurethane
Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material ..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 80 AB Thermoplastic Polyurethane
Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 85 AB Thermoplastic Polyurethane
Introduction: AVALON 85 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 AB is part of the AVALON Performance Range and offers a premium soling ma..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 85 ABX Thermoplastic Polyurethane
Introduction: AVALON 85 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABX is part of the AVALON Perform Range and offers a specially designed,..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 85 AE Thermoplastic Polyurethane
Introduction: AVALON 85 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 85 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 90 AK Thermoplastic Polyurethane
Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane
Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 92 AB Thermoplastic Polyurethane
Introduction: AVALON 92 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 92 AB is part of the AVALON Performance Range and offers a premium soling ma..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 92 AE Thermoplastic Polyurethane
Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 95 AB Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 95 AE Thermoplastic Polyurethane
Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane
Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane
Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi..
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..