Polymer Property : Casting Temperature = 980 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Casting Temperature 980 - 1080 °C
1800 - 1980 °F
Wieland 1101 Wilaform Gold
Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chainsDental
Casting Temperature 980 - 1080 °C
1800 - 1980 °F
Wieland 1401 Wilaform Gold
Hard standard yellow gold alloy. Easily splintered and polished thus very well suited for crafts and industrial decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tu..