Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 5 | 300 °C | 572 °F | Extrusion Coating |
DuPont™ Nucrel® 30705 Ethylene Acrylic Acid Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethyle.. |