Polymer Property : Zone 5 = 338 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 5 316 - 338 °C
601 - 640 °F
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)  (Unverified Data**)
Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th..
Zone 5 316 - 338 °C
601 - 640 °F
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)  (Unverified Data**)
Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous ..
Zone 5 316 - 338 °C
601 - 640 °F
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of..
Zone 5 316 - 338 °C
601 - 640 °F
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion..