Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 360 - 390 °C | 680 - 734 °F | |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |
|||
Zone 4 | 360 °C | 680 °F | Nozzle |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Zone 4 | 360 °C | 680 °F | Nozzle |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Zone 4 | 360 °C | 680 °F | Nozzle |
BASF Ultrason® E 2010 MR HP PESU Description: Unreinforced, medium viscosity standard injection molding grade for improved demolding behavior with Mold Release. PES-Blend with improved processibility. (High Productivity) Abbreviate.. |
|||
Zone 4 | 360 °C | 680 °F | Nozzle |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |