Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Zone 4 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Zone 4 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6 Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au.. |
|||
Zone 4 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Zone 4 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |