Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1155D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 4 | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
LG Chemical KEYFLEX BT GN7155F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Zone 4 | 220 - 240 °C | 428 - 464 °F | Extrusion Molding |
LG Chemical LUPOL GP1007FE Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Zone 4 | 220 - 240 °C | 428 - 464 °F | |
Arkema Group OREVAC® 18319 Grafted Maleic Anhydride Polyethylene OREVAC 18319 is a maleic anhydride grafted polyethylene used in the manufacturing of multi-layer aluminium panels. OREVAC 18319 is mainly used in aluminium panels to have good adhesion performances .. |
|||
Zone 4 | 230 - 240 °C | 446 - 464 °F | Extrusion Molding |
LG Chemical KEYFLEX BT S5035 Ester Type TPE Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide.. |