Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 199 - 221 °C | 390 - 430 °F | |
Ravago Manufacturing Americas Hylac® EX28 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Zone 4 | 199 - 221 °C | 390 - 430 °F | |
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra.. |
|||
Zone 4 | 199 °C | 390 °F | Extrusion |
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and.. |
|||
Zone 4 | 199 °C | 390 °F | Extrusion |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Zone 4 | 199 - 221 °C | 390 - 430 °F | |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Zone 4 | 199 °C | 390 °F | Extrusion |
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, E.. |
|||
Zone 4 | 199 - 210 °C | 390 - 410 °F | |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryerUses: Extrusion: Cable jacket, hose/tube, profile and film and .. |
|||
Zone 4 | 199 °C | 390 °F | Extrusion |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |
|||
Zone 4 | 199 - 204 °C | 390 - 399 °F | Extrusion |
Lubrizol Estane® 58280 Thermoplastic Polyurethane Type: Estane® 58280 is a polyether-type thermoplastic polyurethane (TPU) compound.Features: High resiliency compound, with unique physical properties such as low tensile and compression set, high r.. |
|||
Zone 4 | 199 °C | 390 °F | Extrusion |
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformat.. |
|||
Zone 4 | 199 °C | 390 °F | Extrusion |
Lubrizol Estane® 58437 Thermoplastic Polyurethane Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi.. |