Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 260 °C | 500 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Zone 4 | 260 - 290 °C | 500 - 554 °F | |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Zone 4 | 260 - 290 °C | 500 - 554 °F | |
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,.. |
|||
Zone 4 | 260 - 310 °C | 500 - 590 °F | |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Zone 4 | 260 °C | 500 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Zone 4 | 260 °C | 500 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail.. |
|||
Zone 4 | 260 °C | 500 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Zone 4 | 260 °C | 500 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru.. |
|||
Zone 4 | 260 °C | 500 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Zone 4 | 260 °C | 500 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Zone 4 | 260 °C | 500 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Zone 4 | 260 °C | 500 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Zone 4 | 260 °C | 500 °F | CoExtrusion with Nylon Processing |
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 °C | 500 °F | Nozzle |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Zone 4 | 260 °C | 500 °F | Nozzle |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 °C | 500 °F | Nozzle |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove.. |
|||
Zone 4 | 260 °C | 500 °F | Nozzle |
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT Description: Is a PBT-I, injection-molding grade with 30% glass fibers, for rigid, tough and dimensionally stable technical parts with increased requirements on hydrolysis resistance and toughness, .. |