Polymer Property : Zone 4 = 235 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 215 - 235 °C
419 - 455 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1055D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 4 215 - 235 °C
419 - 455 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3038D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Zone 4 210 - 235 °C
410 - 455 °F
Vent; Extrusion
Kolon DIAMAT® EG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 4 210 - 235 °C
410 - 455 °F
Vent; Extrusion
Kolon DIAMAT® EH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 4 210 - 235 °C
410 - 455 °F
Vent; Extrusion
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 4 210 - 235 °C
410 - 455 °F
Vent; Extrusion
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 4 210 - 235 °C
410 - 455 °F
Vent; Extrusion
Kolon DIAMAT® IG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 4 210 - 235 °C
410 - 455 °F
Vent; Extrusion
Kolon DIAMAT® IH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 4 210 - 235 °C
410 - 455 °F
Vent; Extrusion
Kolon DIAMAT® IM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Zone 4 225 - 235 °C
437 - 455 °F
Injection
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin
Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj..