Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7178 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7399 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7661/RD PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7953 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8290 PPS, linear, with aramid reinforcement Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8400 PPS, linear, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 21-7976 Polyamide 6/6T, with glass fiber and PTFE, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 21-8113 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Zone 3 | 320 - 335 °C | 608 - 635 °F | C3 Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Zone 3 | 320 - 335 °C | 608 - 635 °F | C3 Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Zone 3 | 320 - 335 °C | 608 - 635 °F | C3 Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7629/EG PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7767 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-7869/BL PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Zone 3 | 320 - 335 °C | 608 - 635 °F | C3 Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Zone 3 | 320 °C | 608 °F | Metering-zone |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Zone 3 | 320 °C | 608 °F | Metering-zone |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Zone 3 | 320 °C | 608 °F | Metering-zone |
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Zone 3 | 320 - 335 °C | 608 - 635 °F | |
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8144 PPS, linear, with mineral filler Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low waterabsorbtion.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Zone 3 | 320 - 340 °C | 608 - 644 °F | |
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr.. |
|||
Zone 3 | 320 - 335 °C | 608 - 635 °F | C3 Cylinder Temp for Electronic and Electric Standard Molding |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |