Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66 Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app.. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66 Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara.. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It .. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66 Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a.. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66 Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66 Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66 Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper.. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66 Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Zone 3 | 280 - 295 °C | 536 - 563 °F | |
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66 Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Zone 3 | 270 - 295 °C | 518 - 563 °F | Front Zone |
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Conditioned) Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughnes.. |
|||
Zone 3 | 270 - 295 °C | 518 - 563 °F | Front Zone |
BASF Ultramid® TG3S 15% Glass Filled PA6 (Dry) Description: Ultramid TG3S is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a ba.. |
|||
Zone 3 | 270 - 295 °C | 518 - 563 °F | Front Zone |
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Dry) Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the.. |
|||
Zone 3 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM Vydyne® 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. Vydyne 64C-R resin offers high strength.. |
|||
Zone 3 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, DAM Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h.. |
|||
Zone 3 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
Zone 3 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
Zone 3 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, .. |
|||
Zone 3 | 270 - 295 °C | 518 - 563 °F | Front Zone |
BASF Ultramid® TG3S 15% Glass Filled PA6 (Conditioned) Description: Ultramid TG3S is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a ba.. |
|||
Zone 3 | 270 - 295 °C | 518 - 563 °F | Front Zone |
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Conditioned) Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the.. |
|||
Zone 3 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 66Z Nylon 66, DAM Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug.. |
|||
Zone 3 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and.. |
|||
Zone 3 | 250 - 295 °C | 482 - 563 °F | |
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, DAM Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, .. |
|||
Zone 3 | 270 - 295 °C | 518 - 563 °F | Front Zone |
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Dry) Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughnes.. |