Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 220 - 265 °C | 428 - 509 °F | |
Ovation Polymers Nemcon™ H ABS DP116P ABS ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Zone 3 | 235 - 265 °C | 455 - 509 °F | |
Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6 Description: Nilamid B FR HF is an unfilled, flame retardant NYLON 6 with excellent flow characteristics, outstanding elongation and impact strength and a good thermal performance. Because of its ex.. |
|||
Zone 3 | 245 - 265 °C | 473 - 509 °F | |
Nilit Nilamid B G4 FR HF 20% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G4 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Zone 3 | 255 - 265 °C | 491 - 509 °F | |
Eurostar Star C BX6088 ABS, 20% Carbon Filled, Injection Molding Star C BX06008 is a 20% Carbon Fiber Reinforced ABS Injection Molding ResinInformation provided by Eurostar. |