Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 3 210 - 230 °C
410 - 446 °F
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro..
Zone 3 220 - 230 °C
428 - 446 °F
Celanese Celstran® PEHD-GF40-01 PE-HD, 40% Glass Reinforced  (Unverified Data**)
40% long fiber glass reinforced, High Density Polyethylene40% long fiber glass reinforced High Density PolyethyleneInformation provided by Celanese
Zone 3 210 - 230 °C
410 - 446 °F
Lehmann & Voss LUVOCOM® TPU-7682 Thermoplastic polyurethane, with carbon fiber
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers..
Zone 3 210 - 230 °C
410 - 446 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1055D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 3 210 - 230 °C
410 - 446 °F
Extrusion Molding
LG Chemical LI933 Co-Extrusion ASA
Description: Good Weatherability, Low GlossApplication: Canopy, Siding, Fence, (Roofing) TilesCAS: 26299-47-8Information provided by LG Chemical
Zone 3 210 - 230 °C
410 - 446 °F
Extrusion Molding
LG Chemical LI968W Co-Extrusion ASA
Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical
Zone 3 210 - 230 °C
410 - 446 °F
Extrusion Molding
LG Chemical LI970 Co-Extrusion ASA
Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical
Zone 3 210 - 230 °C
410 - 446 °F
Extrusion Molding
LG Chemical LI970HF Co-Extrusion ASA
Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical
Zone 3 200 - 230 °C
392 - 446 °F
Extrusion Molding
LG Chemical MA210 ABS, Low Gloss
Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Zone 3 220 - 230 °C
428 - 446 °F
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer
Pearlthane® 12H92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and excellent low temperature performance..
Zone 3 210 - 230 °C
410 - 446 °F
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as..
Zone 3 220 - 230 °C
428 - 446 °F
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane
PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application..
Zone 3 210 - 230 °C
410 - 446 °F
Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K..
Zone 3 220 - 230 °C
428 - 446 °F
Injection
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin
Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj..
Zone 3 220 - 230 °C
428 - 446 °F
Eurostar Starglas FF001 HDPE, Glass Fiber Filled
Starglas FF001 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar.
Zone 3 220 - 230 °C
428 - 446 °F
Eurostar Starglas FF004 HDPE, Glass Fiber Filled
Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar.
Zone 3 210 - 230 °C
410 - 446 °F
Arkema Group OREVAC® 18319 Grafted Maleic Anhydride Polyethylene
OREVAC 18319 is a maleic anhydride grafted polyethylene used in the manufacturing of multi-layer aluminium panels. OREVAC 18319 is mainly used in aluminium panels to have good adhesion performances ..
Zone 3 220 - 230 °C
428 - 446 °F
Celanese Celstran® PEHD-GF40-01 PE-HD, 40% Glass Reinforced
40% long fiber glass reinforced, High Density PolyethyleneInformation provided by Celanese
Zone 3 220 - 230 °C
428 - 446 °F
Celanese Celstran® PP-GF30-02 AD 3002 PP, 30% Glass Reinforced
30% long strand glass fiber reinforced polypropyleneInformation provided by Celanese
Zone 3 220 - 230 °C
428 - 446 °F
Celanese Celstran® PP-GF30-02 PP, 30% Glass Reinforced
30% long strand glass fiber reinforced polypropylene30% long strand glass fiber reinforced, chemically coupled polypropyleneInformation provided by Celanese
Zone 3 215 - 230 °C
419 - 446 °F
Celanese RITEFLEX 663 TPC, Unfilled
Riteflex 663 is a nominal 63 Shore D thermoplastic polyester elastomer with medium modulus.Information provided by Celanese
Zone 3 220 - 230 °C
428 - 446 °F
Celanese Celstran® PP-GF30-02 AD 3019 PP, 30% Glass Reinforced
30% long glass fiber reinforced polypropylene - UV stabilizedInformation provided by Celanese
Zone 3 220 - 230 °C
428 - 446 °F
Celanese Celstran® PP-GF30-03-Black PP, 30% Glass Reinforced
30% long glass fiber reinforced, chemically coupled, heat stabilized, Polypropylene BLACKInformation provided by Celanese
Zone 3 220 - 230 °C
428 - 446 °F
Celanese Celstran® PP-GF50-10 PP, 50% Glass Reinforced
50% long fiber glass reinforced, enhanced flow, UV stabilized, PolypropyleneInformation provided by Celanese
Zone 3 220 - 230 °C
428 - 446 °F
Celanese COMPEL PP-GF30-04 PP, Glass Reinforced
Heat Stabilized Polypropylene reinforced with 30% long glass fiberIt is normally not necessary to dry CELSTRAN PP. However, should there be surface moisture (condensate) on the molding compound as a..
Zone 3 205 - 230 °C
401 - 446 °F
Celanese RITEFLEX 655A TPC, Unfilled
Riteflex 655A is a thermoplastic polyester elastomer with nominal shore D hardness of 55 and medium modulus.Information provided by Celanese
Zone 3 220 - 230 °C
428 - 446 °F
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane  (discontinued **)
PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio..
Zone 3 220 - 230 °C
428 - 446 °F
Celanese Celstran® PEHD-GF60-01 PE-HD, 60% Glass Reinforced
58% long strand glass fiber reinforced high density polyethyleneInformation provided by Celanese
Zone 3 220 - 230 °C
428 - 446 °F
Celanese Celstran® PP-GF30-02 AF 3001 PP, 30% Glass Reinforced
30% long glass fiber reinforced polypropyleneInformation provided by Celanese
Zone 3 210 - 230 °C
410 - 446 °F
Extrusion Molding
LG Chemical LI923 Extrusion ASA
Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical