Polymer Property : Zone 3 = 370 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres
Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified
Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber
Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE
Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-7725 VP Polyether sulfone, with glass fiber, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-7939/GY Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8194 Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8301 Polyether sulfone, with carbon fiber, PTFE, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and ..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8326 Polyether sulfone, with carbon fiber, PTFE, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR Polyether sulfone, with glass fiber, easy flowing, demolding aid
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR/BK Polyether sulfone, with glass fiber, easy flowing, demolding aid
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100/GF/30/NAT Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-7337/WT Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-7721/WT9016 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-7890 Polyether sulfone, with carbon fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8049 Polyether sulfone, with glass fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Zone 3 350 - 370 °C
662 - 698 °F
Lehmann & Voss LUVOCOM® 1100-8166 Polyether sulfone, with glass fiber, easy flowing
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..