Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 100 - 120 °C | 212 - 248 °F | Metering |
Lubrizol Advanced Materials Pearlbond® Eco D900 Thermoplastic Polyurethane Pearlbond™ ECO D900 is a linear, aromatic polyurethane based on specialty polyol from renewable sources. It contains 67% of renewable material as certified according to ASTM-D6866. It is suppli.. |