Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 3 = 176 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 3 176 °C
349 °F
Extrusion
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane
Features: Excellent blend partner for PVC and general adhesive and good physical properties.Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating.Available in Americas, Eur..
Copyright © lookpolymers.com All Rights Reserved